Komposisi Kimia

1.4006 KeluliEN 10088-3:2005
Unsur Kimia% Hadir
Karbon (C)0.08 - 0.15
Chromium (Cr)11.50 - 13.50
Silikon (Si)0.0 - 1.00
Mangan (Mn)0.0 - 1.50
Fosfor (P)0.0 - 0.04
Sulfur (S)0.0 - 0.02
Nikel (Ni)0.0 - 0.75
Besi (Fe)Baki

 

Hartanah

Harta FizikalNilai
Ketumpatan7.75 g/cm³
Pengembangan Terma9.9 x 10-6/K
Modulus Keanjalan300 GPa
Kekonduksian Terma24.9 W/m.K
Kerintangan Elektrik0.57 x 10-6Ω.m
Bar - Sehingga 160mm Diameter atau KetebalanEN 10088-3:2005
Harta MekanikalNilai
Bukti Tekanan450 Min MPa
Kekuatan Tegangan650 - 850 MPa
Pemanjangan A15 Min %