What Is ASTM A249 Material Equivalent To?

ASTM A249 covers welded (not seamless) stainless steel tubes made from austenitic grades. The equivalent materials vary based on the specific grade (e.g., TP304, TP316, TP321). Here's a breakdown of common ASTM A249 grades and their equivalent materials in global standards:

ASTM A249 Grade
TP304 S30400 EN 1.4301 / X5CrNi18-10 SUS 304 18/8 Stainless Steel
TP304L S30403 EN 1.4307 / X2CrNi18-9 SUS 304L Low-carbon 304
TP316 S31600 EN 1.4401 / X5CrNiMo17-12-2 SUS 316 Mo-enhanced 304
TP316L S31603 EN 1.4404 / X2CrNiMo17-12-2 SUS 316L Low-carbon 316
TP321 S32100 EN 1.4541 / X6CrNiTi18-10 SUS 321 Ti-stabilized 304
TP347 S34700 EN 1.4550 / X6CrNiNb18-10 SUS 347 Nb-stabilized 304

 

What is the chemical composition of A249?

Chemical Composition Of A249

Chemical Composition Of A249

ASTM A249 Dimensional Tolerances

<= 1/2 inch (12.7 mm) ± 0.005 inch (0.13 mm)
> 1/2 inch to 1 inch ± 0.005 inch (0.13 mm)
> 1 inch to 1-1/2 inch ± 0.006 inch (0.15 mm)
> 1-1/2 inch to 2 inch ± 0.008 inch (0.20 mm)
> 2 inch ± 0.010 inch (0.25 mm)

What is ASTM A249 used for?

→ For heat transfer applications like heat exchangers and condensers.

 

Is ASTM A249 seamless or welded?

→ Welded, often cold-worked to meet dimensional tolerances.

 

What is the difference between A249 and A269?

→ A249 is for heat exchanger service and includes specific testing (e.g. flattening), while A269 is for general corrosion resistance.

 

Is TP316L in A249 the same as in A312?

→ Yes, both use the same material chemistry, but A249 is for and A312 is for .