Keluli Tahan Karat 440C Batang Kecil Cerah
Jan 22, 2026
Tinggalkan pesanan



Gred
| 440C | S44004 | SUS440C | 1.4125 | X105CrMo17 | 95KH18 |
bahan kimia
| C | Mn | P | S | Si | Cr | Mo |
| 0.95-1.20 | 1.00 maks. | 0.040 maks | 0.030 maks | 1.00 maks. | 16.0-18.0 | 0.75 maks. |
Senarai Harga Rod ASTM A276 Type 440C
| Senarai harga Bar Bulat Keluli Tahan Karat 440c di India | 1.4125 AISI 440c SS Senarai Harga Bar (INR) | Harga Rod Keluli Tahan Karat AISI 440c dalam Pound sterling UK | 1.4125 Harga Bar Bulat AISI 440c SS dalam Dirham UAE |
|---|---|---|---|
| DAWAI AISI 440C SEJUK, DALAM BENTUK GEJEL, 7 MM (KELULI TAHAN KARAT) | 370 | 4.00 | 19.07 |
| BAR BULAT KELULI TAHAN KARAT GRED 440C | 61 | 0.66 | 3.14 |
| DIN 1.4125 DIGILAT TANAH, DALAM 3M PANJANG DIAM 20.00MM (JONG KELULI TAHAN KARAT) | 1,959 | 21.19 | 100.99 |
| STAINLESS STEEL HR ROUND BAR GRED 440C | 51 | 0.55 | 2.63 |
Sepasang:Apakah Keluli Tahan Karat 304L
Hantar pertanyaan