AISI 410 410L 410S Keluli Tahan Karat
Jan 22, 2026
Tinggalkan pesanan



Spesifikasi gred bagiAISIKeluli tahan karat gred 410
| Gred | UNS No | British lama | Euronorm | SS Sweden | JIS Jepun | ||
| BS | En | Tidak | Nama | ||||
| 410 | S41000 | 410S21 | 56A | 1.4006 | X12Cr13 | 2302 | SUS 410 |
| 410L | S40977 | – | X2CrNi12 | 1.4003 | X2CrNi12 | – | SUS410L |
| 410S | S41008 | 403S17 | X6Cr13 | 1.4000 | X6Cr13 | 2301 | SUS410S |
ChemikCtentangan
| Gred | C | Mn | Si | P | S | Cr | Ni | |
| 410 | min. maks. |
– 0.15 |
– 1 |
– 1 |
– 0.04 |
– 0.03 |
11.5 13.5 |
0.75 |
| 410L | min. maks. |
– 0.03 |
– 1 |
– 1 |
– 0.04 |
– 0.03 |
11.5 13.5 |
– |
| 410S | min. maks. |
– 0.08 |
– 1 |
– 1 |
– 0.04 |
– 0.03 |
11.5 13.5 |
– 0.60 |
Seterusnya: Apakah Keluli Tahan Karat 304L