EN 1.4841 Plat dan Lembaran Keluli Tahan Karat
Apr 01, 2026
Tinggalkan pesanan



| Standard |
ASTM A240, BS 1449-2, DIN 17440, EN 10088-2, GOST 5632, ISO 9328-7, JIS G4304 |
|---|---|
| Gred |
1Cr25Ni20Si2, 25 20, S31008, SUS310S, X8CrNi25-21 (1.4845) |
| Panjang |
2000mm – 6000mm (78.7in – 236.2in), Disesuaikan |
| Ketebalan |
3mm – 100mm (0.12in – 3.94in), Disesuaikan |
| Lebar |
1000mm – 2000mm (39.4in – 78.7in), Disesuaikan |
| Kemasan Permukaan |
BA, HL, Cermin, No.1, No.2B, No.4, Jeruk |
| Teknik |
Canai Sejuk, Canai Panas |
| Borang |
Gegelung 310/310/310H, Plat Berkotak-kotak 310/310S/310H, Plat Berlubang 310/310S/310H, Jalur 310/310S/310H, Kemasan BA 310/310S/310H Helaian 310/310S/310H, Plat Panas 310S/310H Lembaran Selesai 310/310S/310H Digulung/Sejuk, Lembaran Kemasan Cermin 310/310S/310H, Plat Kemasan No.1 310/310S/310H, Lembaran Kemasan No.2B 310/310S/310H, Lembaran Kemasan No.103/310H, Lembaran No.110S/310H |
Syarat Perniagaan
| Syarat | Spesifikasi |
|---|---|
| Kuantiti Pesanan Minimum: | 5 Tan |
| Harga: | Untuk dirundingkan |
| Butiran Pembungkusan: |
Seperti yang Diminta |
| Masa penghantaran: | Dalam 7-10 Hari Bekerja |
| Syarat Pembayaran: | T/T, L/C, Kad Kredit |
| Keupayaan Bekalan: | 100000 tan sebulan |
| Pensijilan: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Eksport Ke: |
Amerika Syarikat, India, United Kingdom, Turki, Kanada, Afrika Selatan, Australia, Korea, Brazil, India, Indonesia, Malaysia, Persekutuan Rusia, dsb. |
Hantar pertanyaan